What Is Sheet Metal

What is sheet metal

Many factories have been making these mistakes repeatedly over the past decade or so, such as inaccurate dimensions of sheet metal parts, burrs left on the surface, or deformation after welding. In response to these problems, the person in charge of the production line suggested that everyone take out the quality control points in these six links and compare and inspect them one by one.

Incoming board materials are the first step

When the cold-rolled plate, stainless steel or aluminum plate arrives, the first thing to do is to check the thickness deviation, whether there are any scratches on the surface, and the material list.

In 2024, an automobile factory encountered such a situation. The plates they used were marked as 8 mm thick, but were actually only a little over 7 mm. As a result, the rebound of the entire batch of bent parts was uncontrollable, and the final scrap cost exceeded 800,000 yuan.

The batch number of each batch of raw materials entering the factory must be clear, and the name of the supplier must be written down. By the way, the material certificate must also be kept. Once the product is unqualified, it must be placed in a separate place for isolation and storage. Aluminum plates are particularly afraid of scratches. If there is only a very small trace on an aluminum plate as thin as 0.5 mm, it cannot be hidden under the light after spraying powder. Customers can see it at a glance and will directly consider it as a return.

Keep an eye on the mold gap during the stamping process

The gap of the mold is set according to 8% to 10% of the plate thickness. For a plate with a thickness of 3 mm, the corresponding gap range should be 0.24 mm to 0.3 mm. If the gap is set too small, edge chipping will easily occur. If the gap is set too large, the burrs will exceed the specified standard. During the stamping operation, after every 500 products are punched, one piece must be taken to check the cross section. If it is found that the burr value exceeds 0.2 mm, the machine should be stopped immediately and the mold should be adjusted.

钣金加工质量控制点_钣金加工工艺 冷轧板不锈钢铝板表面处理 爱采购钣金件采购

There is a manufacturer in Dongguan that produces chassis. In the year 2025, it did not conduct the required regular sampling inspections. When the customer inspected the goods, they found that the burr rate was as high as 12%. As a result, the entire batch of goods was returned, and more than 400,000 yuan was paid in liquidated damages to pay fines. When the service life of the mold has reached the end , the sheet metal processing quality control points are not repaired, resulting in dimensional deviations that occur silently.

The bending angle must be considered as rebound

The rebound angle of stainless steel 304 is between 1.5 degrees and 2 degrees, and the aluminum plate can reach more than 3 degrees. Therefore, before performing the bending operation, the sample must be folded first, and then the mold must be adjusted as needed. The V-groove needs to match the thickness of the plate. If it is a 3mm thick plate, a 30mm-wide groove must be used for processing. If a 20mm groove is mistakenly used, the bottom of the plate will be directly cracked.

After the folding action is completed, a 90-degree test sample must be used immediately for comparison and inspection. If the measured deviation exceeds 0.5 degrees, the relevant parameters need to be reset. For relatively precise components such as elevator cars, as long as there is a half-degree difference in angle, the door gap will become so narrow that even the sealing strip cannot be inserted, ultimately making it impossible to perform installation work on site.

Don’t break the welding shape hard

When multi-point welding is performed on 0.5mm thin plates, it is easy to cause warping and deformation of the workpiece. Therefore, the length of the single-pass weld must be strictly controlled within 50mm, and jump welding method should be used to disperse the stress generated.

After all these are welded, use a feeler gauge to measure where the weld is stuck. If the gap is found to be more than 0.3mm, it will be directly regarded as a defective product and must not be dealt with by hammering or forcibly breaking it.

The process cost of CO2 welding is about 40% less than that of argon arc welding, but the number of pores produced by this method is relatively high. For key components that are stressed, this method must not be used just to save money. Tensile testing is required for each batch. If it is found that the yield strength does not reach more than 90% of the material standard value, the entire batch of products must be pulled back and reprocessed.

钣金加工工艺 冷轧板不锈钢铝板表面处理 爱采购钣金件采购_钣金加工质量控制点

The surface treatment depends on the thickness but not the color.

The thickness of the powder coating is set between 60 microns and 80 microns. If this value is lower than 50 microns, the corrosion resistance cycle time will be cut in half. The national standard for electroplated zinc layer has been adjusted in 2025, and the minimum standard is 8 microns. When testing ordinary parts, the salt spray test requires 96 hours to ensure that no red rust appears. For parts used in automobiles, this indicator requires 500 hours.

Within forty-eight hours after powder spraying, the product must be avoided from being exposed to the sun. Otherwise, the adhesion will decrease and the probability of peeling at the corners will triple. After electroplating, it is necessary to carefully check whether there is any hydrogen embrittlement problem. For those parts made of high carbon steel, if the hydrogen removal treatment is not performed within forty-eight hours, they may break after two weeks.

Go through final inspection before shipment

Dimensional tolerances must comply with the drawings, the surface must not be scratched or oxidized, and packaging must be anti-collision measures. If any one of these three requirements is missing, it will not be released. If the diagonal deviation of the distribution cabinet shell exceeds 1 mm, the hinge cannot be installed, and the cost of rework at the construction site is five times more expensive than rework in the factory.

The inspection report must be attached when the goods are delivered, and the batch information, relevant test data, and treatment records for unqualified items must be clearly marked in the report . Sheet metal processing quality control point . Sheet metal processing quality control point . What is sheet metal? Because in the incident that occurred in a certain elevator factory in 2025, they had to recall three car doors because they missed the specific batch number, which stopped the entire production line for two weeks. This ultimately led to the customer directly withholding the framework order for that quarter.

May I ask, in your production line, which stage of quality control is most likely to cause problems? Welcome to discuss in the message area. If you think this information is of practical value, please give it a thumbs up and forward it to the person in charge of the workshop for reference.