How to effectively repair car iron rust problem?
Once the iron sheet on the car body is rusted, many people will just throw the car away and buy a new one. However, in 90% of the cases, it can be repaired for dozens of dollars, which can save a lot of money. This money is enough to eat several good meals. The key point in this situation is actually to see how serious the rust is.
Surface rust can be solved with sandpaper
The rust spots appeared at the beginning. The color is a little red and a little brown. The area is very small, no more than the size of a fingernail. At this time, you can use the 400-grit water sandpaper to dip it in clean water and grind it repeatedly. It will take about three to five minutes to grind away all the rust, and the original silver-white iron sheet underneath will be exposed.
After the polishing work is completed, be sure to wipe off all the excess water with a dry cloth immediately, and then spray a thin layer of anti-rust primer. Do not wait until the next day to do this step, which will have to be delayed. You must know that in areas with southern climate characteristics such as Chongqing and Hunan, if the surface of the iron sheet is left exposed for more than one night, new rust spots will quickly appear again, so when dealing with it, The speed of movement must be as fast as possible.
Large areas of peeling paint need to be removed and putty added
The rust has spread to several centimeters, and in some cases even covers a larger area. Large areas of bulges and peeling have appeared on the paint surface. Just relying on sandpaper to polish can no longer solve the actual problem. You must use a scraper or angle grinder to completely remove the rust layer and paint layer on the surface until the metal surface shows a bright iron appearance. When removing, pay special attention to the edge processing. It is necessary to adopt a slow transition method to avoid leaving uneven step-like traces after the work is completed.
First shovel the area clean, and then paint it with phosphating primer. The purpose is to lock the iron surface and prevent it from rusting again. Next, use gray putty to scrape on two to three layers.

After each layer is scraped, you must wait twenty-four hours for it to dry completely before scraping the next layer. After all the putty layers are completed, use 800-grit sandpaper to smooth the entire surface.
The rust has penetrated the iron sheet and has to be dug out and re-welded
Fingers can directly penetrate the iron sheet, which shows that the corrosion has become very serious and has destroyed the metal structure, so this piece of material has been completely useless. You need to use a welding gun or plasma cutting machine to cut off the rusted parts in one piece. When cutting, be sure to leave two to three millimeters of rust-free metal on the edges to ensure that there are no traces of rust on the cut surface.
You need to cut out a piece of tinplate first. The size of the patch must be exactly the same. Then you use it to weld, you can choose to use spot welding, or you can choose to use secondary welding. You have to weld all the way along that cut edge, and you have to weld three turns.
When welding, you need to control the distance between solder joints within five millimeters. After the welding is completed, you need to get a whetstone and smooth out all the welding flashes. After this treatment, no protrusions or burrs are allowed to be left on the surface.
Anti-rust treatment after welding is indispensable
The weld is the weakest part of the entire iron sheet. Immediately after welding, use a copper wire brush to clean off all the welding slag, and then spray it with epoxy zinc-rich primer. The natural drying time should be at least six hours. Don't rush to the next step when the air humidity is high on rainy days.
After the primer is completely dry, scrape the putty in order to level the position of the weld, and then spray the midcoat twice to fill in all the tiny blisters. If you choose to cut corners in this step, there will be blooming and graining when the topcoat is sprayed later, and when viewed under the sun, the surface will feel unsuitable no matter how you look at it.

How to align touch-up paint color and gloss
When it comes to touch-up paint, the most troublesome thing is the color difference. When the car body uses dark paint or metallic paint, this difference will be particularly obvious. It is recommended to go to a car repair shop and take out the color card for comparison. The paint code of vehicles of the same model is usually printed on the safety label on the B-pillar, so directly reporting the paint color number is the most accurate way. Do not rely on personal feelings to make a choice.
The spray gun should be kept 20 to 25 centimeters away from the car body, and spray it thinly three to four times. This will be much more uniform than spraying it thickly at once. Finally, wait for forty minutes and then cover it with a layer of the same type of varnish. Then the gloss level and the feeling of the original paint next to it will be basically the same.
Daily rust prevention is more important than rust repair
Every year before summer, I spend two to three hundred yuan to spray chassis armor on the chassis and wheel arches. If you do this, it will be much more cost-effective than having to spend thousands of dollars to repair the rusted parts in the future. Car owners in places like Sichuan and Hunan need to be especially worried, because the air there is relatively humid all year round, so the iron sheet ages and deteriorates twice as fast as here in the north.
Everyone who has just run on a snowy road in winter, or just driven out of a mud pit, must get home that night, quickly pick up the water pipe, and wash the chassis of the car carefully. Don't wait until the mud is dry and caked in the iron gaps of the vehicle before dealing with it. You must know that these narrow gaps are an extremely favorable breeding ground for corrosion. If the situation is allowed to develop, it will not take that long at all. In other words, within a year and a half, it is very likely that the entire metal part of the vehicle floor will be completely rusted through.
At what stage has the rust on the body shell of your car reached? Are sporadic red dots just beginning to appear, or is it so severe that you can poke holes directly with your fingers? Feel free to leave a message in the comment area for discussion. If you find this answer useful, please click the like button and forward it to your friends and car enthusiasts who drive old vehicles.












No comments yet