Dimensional Tolerance And Welding Performance Of HEM120 European Standard H-shaped Steel

Dimensional tolerance and welding performance of HEM120 European standard H-shaped steel

The heavy H-shaped steel was transported to the construction site. As a result, there was a deviation of more than one millimeter or hysteretic damage cracks occurred at the bottom of the flange. As a result, the cost of reprocessing exceeded the money spent on purchasing materials. The reason for this situation is that the allowable error range and the specific welding operation method are not well coordinated and coordinated. Therefore, no matter how thick the thickness of the wing plate is increased, It cannot withstand the dynamic pressure load during use.

How to fix the section thickness tolerance?

The nominal thickness of the HEM140 web is 12.5mm, which implements +10%/-5% asymmetric tolerance control. The flange thickness is 21mm, which corresponds to a +10%/-3% tolerance range.

The actual thinnest part of the web shall not be less than 11.9mm, and the actual thinnest part of the flange shall not be less than 20.3mm. The dimensional tolerance and welding performance of the HEM120 European standard H-shaped steel, which is cut according to symmetrical tolerances when blanking, when the web is locally thinned by 0.6mm, the section modulus will directly decrease, causing the stress concentration under heavy load to exceed the standard limit.

The weight deviation of the same batch of deliveries is controlled within the range of plus or minus 4%. This indicator exactly matches the European norm standard 10034 for the allowable error of heavy-duty steel.

Therefore, in the logistics calculation work and cost accounting process, it is enough to calculate according to the theoretical weight, and there is no need to carry out separate weighing operations. When the European Union updates its high-intensity connection specifications in 2026, it will also require these deviation indicators to be tightened in this established direction.

Shape and position accuracy determines whether the hole position is correct or not

The sag value of the curvature of each meter of web must be controlled and reduced to a threshold of 0.3 mm. For an overall length of 12 meters, the total straightness deviation must not exceed the limit of 4 mm. The parallelism error on the outside of the flange must be controlled within 0.8 mm, and the deviation of the inclination angle must also be maintained within the standard range of one percent.

Unfortunately, because defects such as side bending, twisting, and flange deflection have not been completely solved, the high-strength bolt hole alignment work is performed on site and requires manual trimming.

HE120M_Copy.jpg

尺寸公差体系EN 10034_建筑钢结构中厚板H型钢下料铆焊_HEM120欧标特厚翼缘重载H型钢

Entering 2026, the new regulations and standards introduced by the European Union have stricter regulations on the allowable deviation values ​​of high-strength connection holes. Once the shape and position accuracy cannot meet the established standards, it will be directly judged as unqualified.

In the process of the processing workshop, after the blanking process is completed, inspection tools need to be used first to select and screen out parts with bending and twisting problems. The advantage of this is that it is much cheaper than waiting for the components to be transported to the construction site and then going back to rework and repair them. It can save about ten times the cost.

Cut to length and end cuts

The conventional 6-meter and 12-meter fixed-length tolerances are ±50mm, and high-precision assembly-level orders are received with ±10mm. The end face is CNC sawed, the bevel angle is ±1.5°, the roughness Ra does not exceed 25μm, and there is no burr larger than 1mm. Workers receive the materials and directly connect them, saving one polishing process and half a day of construction time.

When performing riveting and welding blanking operations, everyone must pay attention to the fact that the slope of the end face must be consistent with the docking angle specified on the product drawing. If the cutting is off-center, it is easy to leave pores at the root of the weld.

Therefore, the workshop can prepare several sawing templates with different angle specifications as reference standards. After each batch of materials is cut, two workpieces need to be randomly selected for inspection. Compared with the comprehensive inspection method, this method is faster and can also save the wear and tear of the grinding wheel.

Carbon equivalent control is the key to thick flange welding

This material belongs to S355 material, and its carbon equivalent CEV needs to be strictly controlled under 0.42%. In this state, as long as it is in a normal temperature environment, even using the two welding materials E50 electrode or ER50 welding wire, it is fully capable of completing conventional welding operations, and the strength of the weld is stable, and it can fully cover the strength requirements of the base metal. However, because the thickness of the flange part has reached a specification of 21mm, And the range of the heat affected zone will exceed 25mm, so at this time, the preheating step must ensure that the temperature reaches the degree range of 120 to 150 degrees Celsius. At the same time, the control of the heat input is also extremely strict, and it must be stuck within the upper limit of 25kJ/cm.

Multi-layer and multi-pass welding is a hard requirement for thick flange welding, because if single-pass welding is used, the heat input will be relatively concentrated, and delayed cracks at the flange root will still appear and become apparent after two weeks. Regarding the welding of dissimilar steel materials, there is no problem in joining S355 material and Q355 material together. The preheating temperature and heat input parameters can be selected according to the thicker side, so as to ensure that the mechanical properties of the joint remain stable.

Don’t be lazy about post-weld stress treatment

建筑钢结构中厚板H型钢下料铆焊_尺寸公差体系EN 10034_HEM120欧标特厚翼缘重载H型钢

For situations such as heavy-duty equipment supports and bridge load-bearing components that work under dynamic loads, they cannot be delivered directly for use after welding is completed. These things must be heated as a whole to a temperature within the range of 580±10°C, then maintained for two hours, and then slowly cooled down with the furnace. After doing this, the residual stress can be reduced to less than one-third of the yield strength of the base material, and the fatigue life can be increased.

For small components, since there are no objective conditions for entering the furnace for overall heat treatment, we need to implement at least local post-weld heat treatment. Specifically, we need to bake the 50 mm width on both sides of the weld to the same temperature level as the weld itself.

If we omit this very critical process of blanking and riveting the H-shaped steel plates in the building steel structure, then after three years, once it is subjected to the impact of dynamic loads, cracks will first appear at the point where the stress is concentrated, which will lead to the complete scrapping of the entire beam.

Tolerance welding collaboration is the real deal

The two indicators of flange parallelism and straightness are fixed to death, so that the amount of docking misalignment is always within the range of less than or equal to 1mm, and at the same time, it is ensured that the assembly gap does not exceed the standard value. In this way, problems such as welding deformation and stress concentration are eliminated directly from the source.

The purpose of adopting asymmetric thickness design is to ensure that the actual thickness of the web and wing ribs is definitely not less than the specified lower limit value, so as to ensure that the welded joint part will never become a weak link in the entire structure.

Only by combining these two aspects can we truly meet the requirements of EN 1993 for overloaded components. Before the cutting step, the tolerance drawing and welding process card need to be sent to the production workshop, and then the riveters and welders will perform construction according to this card. This method is much more reliable than welding and measuring dimensions at the construction site.

The latest riveting and welding operation of H-shaped steel in your workshop was performed because the tolerance indicator was not well controlled, or because there were no errors in the welding parameters. You can go to the comment area to chat. If you think this content is useful, please click like and forward this information to the riveting welding master.

© Copyright Notice
THE END
喜欢就支持一下吧
Likes9 Share
评论 Be the First to Comment

Please log in to comment